PTFE is a material subject to plastic flow. When cycled through heat and then cooled down in process lines,
PTFE gaskets will not return to the original configuration and it will continue to compress as the cycling
continues. This plastic flow will allow leakage if clamp torques are not maintained.
Features:
color code: red dot
10 mesh standard, other mesh available-call for details
meets 21CFR 177.2600
Clamp Gaskets
Features:
color code: FKM usually not marked
peroxide cured FKM
meets 21CFR 177.1550
PTFE passed USP Class VI Cytotoxicity testing
Features:
color code: usually not marked
peroxide cured EPDM
meets 21CFR 177.1550
PTFE passed USP Class VI Cytotoxicity testing
PTFE Envelope Clamp Gaskets with FKM Filler
PTFE Envelope Clamp Gaskets with EPDM Filler
Features:
color code: pink dot
peroxide cured
meets 21CFR 177.2600
passed USP Class VI Cytotoxicity testing
not recommended for use with bolted clamps
Type 2 - Flanged
1" and larger
Silicone Flanged Clamp Gaskets -
White
Buna-N Mesh Screen Clamp Gasket, 316
Size
Part #
Price/E
1"
40MPF-XW100
$4.75
1½"
40MPF-XW150
4.95
2"
40MPF-XW200
4.95
2½"
40MPF-XW250
6.15
3"
40MPF-XW300
7.35
4"
40MPF-XW400
9.70
6"
40MPF-XW600
51.50
8"
40MPF-XW800
64.05
10"
40MPF-XW1000
79.85
12"
40MPF-XW1200
82.15
Size
Part #
Price/E
1"
40MPS-U100
$47.10
1½"
40MPS-U150
41.45
2"
40MPS-U200
44.35
2½"
40MPS-U250
58.85
3"
40MPS-U300
67.75
4"
40MPS-U400
105.95
Size
Part #
Price/E
½"
42MP-GRE50
$15.80
1"
40MP-GRE100
8.65
1½"
40MP-GRE150
7.25
2"
40MP-GRE200
8.10
2½"
40MP-GRE250
9.80
3"
40MP-GRE300
11.45
4"
40MP-GRE400
21.10
6"
40MP-GRE600
74.00
Size
Part #
Price/E
1"
40MP-GR100
$7.85
1½"
40MP-GR150
7.25
2"
40MP-GR200
8.25
2½"
40MP-GR250
10.85
3"
40MP-GR300
11.45
4"
40MP-GR400
19.50
6"
40MP-GR600
93.30
See pages 431-432 for sizing charts.
Type 3 - Mesh
PTFE is a material subject to plastic flow. When cycled through heat and then cooled down in process lines,
PTFE gaskets will not return to the original configuration and it will continue to compress as the cycling
continues. This plastic flow will allow leakage if clamp torques are not maintained.