Torque to Achieve Bolt Utilization 061207
2350 Campbell Road
FAX: 937-498-7544 Admin.
Sidney, OH 45365-9573
FAX: 937-498-4911 Sales
Torque to Achieve Bolt Utilization
(Unlubricated Bolts)
Nominal
Diameter
(in.)
SAE J429
Grade 5
(ft-lbf)
SAE J429
Grade 8
(ft-lbf)
ASTM A193
Grade B7
(ft-lbf)
ASTM A193
Grade B8 (304SS)
(ft-lbf)
Yield
50%
70%
50%
70%
50%
70%
50%
70%
1/4
9
12
12
17
10
14
3
4
5/16
17
24
25
34
20
28
6
9
3/8
30
42
42
59
33
47
11
15
7/16
45
65
66
92
53
74
17
23
1/2
75
105
105
145
84
120
27
37
9/16
105
150
150
210
120
165
38
53
5/8
145
205
205
290
165
230
53
74
3/4
255
360
360
505
290
405
92
130
7/8
410
575
575
805
460
645
150
205
1
615
860
860
1205
690
965
220
310
The ability of a gasket material to make and maintain a seal depends not only on the quality of
the gasket material, but also on medium being sealed, the flange design, the amount of
pressure applied to the gasket by the bolts and how the gasket is assembled into the flanges