SBR Binder Gasketing
KLINGERSIL® C-6400
• Synthetic Fiber
• SBR Binder
• Good Anti-Stick Properties
• Good Steam Sheet
Typical values refer to 1/16" material
unless otherwise specified.
See graphs for temperature & pressure limits
Creep Relaxation
ASTM F38B (1/32")
20%
Sealability
ASTM F37A (1/32")
<0.20 ml/hr
Gas Permeability
DIN 3535/6
<0.3 ml/min
Compressibility
ASTM F36J
8%
Recovery
ASTM F36J
50% minimum
Klinger Hot Compression Test
Thickness Decrease 73°F (23°C)
12% initial
Thickness Decrease 572°F (300°C)
11% additional
Weight Increase
ASTM F146 after immersion in Fuel B
5h/73°F (23°C)
25% maximum
Thickness Increase
ASTM F146 after immersion in
ASTM Oil 1, 5h/300°F (149°C)
0-10%
ASTM Oil IRM903, 5h/300°F (149°C)
10-25%
ASTM Fuel A, 5h/73°F (23°C)
0-5%
ASTM Fuel B, 5h/73°F (23°C)
0-10%
Dielectric Strength
ASTM D149-95a
16 kV/mm
ASTM F104 Line Call Out
F71341B3E42K6M5
Leachable Chloride Content
FSA Method (Typical)
200 ppm
Density
ASTM F1315
112 lb/ft 3 (1.8 g/cc)
Color
(Top/Bottom)
White or Black
Pressure & Temperature Graphs